NON - ASBESTOS JOINTING SHEETS

HNA-600

MATERIAL COMPOSITION:

Aramid Fibre, Glass Fibre, NBR, High Media Resistance, High Stress Condition.

Diagram

Technical Specifications:
Properties Test Method Unit Specified Value
Density gm/cm3 1.70-2.00
Tensile Strength
(a) ACC to ASTM F 152 (Across Grain) N/mm2 >8
(b) ACC to DIN 52910 (Across Grain) N/mm2 >5
Compressibility ASTM F36A % 7-15
Recovery ASTM F36A % >50
Fluid Absorption ASTM F146
(a) In ASTM Oil No. 3
Increase in Mass
Increase in Thickness

%
%

<10
<10
(b) In Fuel B
Increase in Mass
Increase in Thickness
ASTM F146
%
%

<10
<10
(c) In Water/Antifreeze
Increase in Mass
Increase in Thickness
ASTM F146
%
%

<15
<10
Ignition Loss DIN 52911 % <30
Sealability Against Nitrogen DIN 3535 CM3/min <1.0
Stress Resistance
16h 300 oC DIN 52913 N/mm2 25
16h 175 oC DIN 52913 N/mm2 30
Max. Peak Temperature oC 440
Max. Continuous Temperature oC 250
Max. Operating Pressure Kg/CM2 100