Properties | Test Method | Unit | Specified Value |
Density | gm/cm3 | 1.70-2.00 | |
Tensile Strength | |||
(a) ACC to ASTM F 152 (Across Grain) | N/mm2 | >8 | |
(b) ACC to DIN 52910 (Across Grain) | N/mm2 | >6 | |
Compressibility | ASTM F36A | % | 7-15 |
Recovery | ASTM F36A | % | >50 |
Fluid Absorption | ASTM F146 | ||
(a) In ASTM Oil No. 3 Increase in Mass Increase in Thickness |
% % |
<10 <8 |
|
(b) In Fuel B Increase in Mass Increase in Thickness |
ASTM F146 | % % |
<10 <7 |
(c) In Water/Antifreeze Increase in Mass Increase in Thickness |
ASTM F146 | % % |
<10 <7 |
Ignition Loss | DIN 52911 | % | <30 |
Sealability Against Nitrogen | DIN 3535 | CM3/min | <0.5 |
Stress Resistance | – | ||
16h 300 oC | DIN 52913 | N/mm2 | 20 |
16h 175 oC | DIN 52913 | N/mm2 | 30 |
Max. Peak Temperature | oC | 450 | |
Max. Continuous Temperature | oC | 350 | |
Max. Operating Pressure | Kg/CM2 | 100 |
Graphite coating, teflon coating, antistick coating are also available on request. Properties applicable for 2.0mm thick material
43 KM Stone, Delhi-Rohtak Highway,
NH-10, Village Rohad, Dist. Jhajjar,
Bahadurgarh – 124501, Haryana, India
Mobile : +(91)-98110-20116
Telephone : +(91)-1276-278310, 278311
Fax : +(91)-(11)-25885741, 25888090
© 2021 Charminar Jointings | Developed by Mush